Effect of Self-Cured and Self-Etch Adhesive Systems on Shear Bond Strength After Photodynamic Therapy and Disinfection with Different Types of Lasers
dc.contributor.author | Çeşme, Ayşe | |
dc.contributor.author | Hubbezoğlu, İhsan | |
dc.date.accessioned | 2025-05-04T16:25:06Z | |
dc.date.available | 2025-05-04T16:25:06Z | |
dc.date.issued | 2023 | |
dc.department | Sivas Cumhuriyet Üniversitesi | |
dc.description | DIS290 | |
dc.description.abstract | Effect of Self-Cured and Self-Etch Adhesive System on Shear Bond Strength After Photodynamic Therapy and Disinfection with Different Types of Lasers Ayşe Çeşme1-a*, Ihsan Hubbezoğlu1-b 1 Sivas Cumhuriyet University, Faculty of Dentistry, Department of Restorative Dentistry Sivas, Türkiye. ABSTRACT Objectives: The aim of this study was to investigate the strength of shear bonding of self-cured and self-etch adhesive systems to dentin after surface disinfection with Photodynamic Therapy (PDT), Er:YAG, Nd:YAG, and KTP laser. Materials and Methods: In the study, 6 main-groups were formed as Control, Er:YAG Laser, Nd: YAG Laser, KTP Laser, KTP Laser activated PDT and Diode Laser activated PDT. Each group was divided into two subgroups; Self-cured (Tokuyama Universal) and self-etch (Scotchbond Universal) adhesive system(n=10). 120 molar teeth were prepared to expose dentin surfaces. After disinfection and adhesive application, nanohybrid composite resin with a diameter of 3 mm and a height of 2 mm was applied to the dentin surface with the help of transparent molds. All samples were thermally cycled 5.000 times at 5°C and 55°C. Shear bond strength (SBS) test was applied to the samples in a universal test device. Results: The differences between the Er:YAG laser group and the control, KTP and Nd:YAG laser groups of the self-cured adhesive samples were statistically significant. While the differences between the Nd:YAG laser group and the PDT groups were statistically significant (p | |
dc.description.abstract | [No abstract available] | |
dc.description.sponsorship | CUBAP | |
dc.identifier.doi | 10.7126/cumudj.1299029 | |
dc.identifier.doi | https://doi.org/10.7126/cumudj.1299029 | |
dc.identifier.endpage | 172 | |
dc.identifier.issn | 1302-5805 | |
dc.identifier.issn | 2146-2852 | |
dc.identifier.issue | 2 | |
dc.identifier.startpage | 164 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12418/32705 | |
dc.identifier.volume | 26 | |
dc.language.iso | en | |
dc.publisher | Sivas Cumhuriyet Üniversitesi | |
dc.relation.ispartof | Cumhuriyet Dental Journal | |
dc.relation.publicationcategory | Makale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanı | |
dc.rights | info:eu-repo/semantics/openAccess | |
dc.snmz | KA_DergiPark_20250504 | |
dc.subject | photodynamic therapy | |
dc.subject | self-cured adhesive | |
dc.subject | laser disinfection | |
dc.subject | bond strength | |
dc.title | Effect of Self-Cured and Self-Etch Adhesive Systems on Shear Bond Strength After Photodynamic Therapy and Disinfection with Different Types of Lasers | |
dc.type | Research Article |