Browsing Araştırma Çıktıları by Subject "nanoindentation"
Now showing items 1-2 of 2
-
Determination of mechanical properties of polymeric microspheres used in controlled drug delivery systems by nanoindentation
(TAYLOR & FRANCIS INC, 2019)In this study, we synthesized poly (vinyl acetate-co-divinyl benzene) microspheres with various monomer/cross-linker contents for oral/topical sustained drug release applications and determined the micromechanical properties ... -
Nanomechanical Characterization of Flowable Dental Restorative Nanocomposite Resins Using AFM
(TAYLOR & FRANCIS INC, 2017)In this study, exploring the possible connections between the structure and the functionality of a dental restoration material on the sub-micrometric scale is aimed, especially by focusing on the elastic mechanical properties ...