Surface oxygen generated upon N2O activation on iron containing ZSM-5 type zeolites with different elemental composition

Küçük Resim Yok

Tarih

2012

Yazarlar

Ates, Ayten
Reitzmann, Andreas
Waters, Gerrit

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

ELSEVIER SCIENCE BV

Erişim Hakkı

info:eu-repo/semantics/closedAccess

Özet

Various ZSM-5 zeolites with iron contents ranging from of 0.86 to 4.98 and Si/Al ratios of 11.5-140 were prepared by solid-state ion exchange with FeCl2. The catalysts were characterised by XRD, H-2-TPR and NH3-TPD. The formation and stability of surface oxygen over these zeolites were investigated with a transient multipulse technique combined with subsequent temperature-programmed desorption (TPD). Higher iron contents enhance the formation of surface oxygen. However, when a critical iron content is reached, larger iron oxide clusters and particles are formed and these larger clusters do not contribute significantly to surface oxygen formation. Moreover, the amount of desorbed oxygen is more than that formed from N2O due to the additional desorption of oxygen present in the lattice of such oxide clusters. TPD studies indicate the presence of different surface oxygen species depends on both the zeolite iron content and Si/Al ratio. (C) 2012 Elsevier B.V. All rights reserved.

Açıklama

Anahtar Kelimeler

Nitrous oxide decomposition, Fe-ZSM-5, Multipulse method, Surface oxygen