THE EFFECT OF DIFFERENT ACID TREATMENTS ON SHEAR BOND STRENGTH BETWEEN MONOLITHIC ZIRCONIA AND DENTIN SURFACE

dc.contributor.authorUlgey, Melih
dc.contributor.authorGorler, Oguzhan
dc.date.accessioned2024-10-26T17:51:20Z
dc.date.available2024-10-26T17:51:20Z
dc.date.issued2021
dc.departmentSivas Cumhuriyet Üniversitesi
dc.description.abstractObjective: The aim of this study is to evaluate the effect of dentin surface treatments with citric, tartaric, phosphoric, and boric acids on the bonding strength of monolithic zirconia. Materials and Methods: A hundred human molar teeth were randomly divided into subsets (n=10) based on acid treatment modalities and thermocycling procedure. Monolithic zirconia superstructures were fabricated using CAD/CAM system in the final dimensions of 7 mm in diameter and 3 mm in thickness. After application of acid treatments to dentin surface, shear bond strength test was performed to assess the effectiveness of surface modifications that were also examined using a scanning electron microscope. Results: The study groups were ranked respectively as (citric acid>tartaric acid>phosphoric acid>boric acid>control) for the set of groups without thermocycling and (citric acid>tartaric acid) and (phosphoric acid>boric acid>control) for the set of thermocycling groups (p<0.05) based on highest value. The bonding strength of tartaric acid group was not significantly different from the bonding strength of phosphoric acid group (p>0.05). Conclusions: In both procedures with and without thermal cycling; based on order of efficacy, citric, tartaric, phosphoric, and boric acids were more effective in improving the shear bond strength between monolithic zirconia and dentin surface. The thermal cycling procedure decreased the bonding strength in all the groups. © 2021, Cumhuriyet Dental Journal. All Rights Reserved.
dc.description.sponsorshipScientific Research Projects Commission; Sivas Cumhuriyet Üniversitesi, (DIS-188)
dc.identifier.doi10.7126/cumudj.804149
dc.identifier.endpage9
dc.identifier.issn2146-2852
dc.identifier.issue1
dc.identifier.scopus2-s2.0-85143867054
dc.identifier.scopusqualityQ4
dc.identifier.startpage1
dc.identifier.trdizinid1109197
dc.identifier.urihttps://doi.org/10.7126/cumudj.804149
dc.identifier.urihttps://search.trdizin.gov.tr/tr/yayin/detay/1109197
dc.identifier.urihttps://hdl.handle.net/20.500.12418/26171
dc.identifier.volume24
dc.indekslendigikaynakScopus
dc.indekslendigikaynakTR-Dizin
dc.language.isoen
dc.publisherCumhuriyet University Faculty of Dentistry
dc.relation.ispartofCumhuriyet Dental Journal
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectBoric acid; Citric acid; Dentin; Phosphoric acids; Shear strength; Zirconium oxide
dc.titleTHE EFFECT OF DIFFERENT ACID TREATMENTS ON SHEAR BOND STRENGTH BETWEEN MONOLITHIC ZIRCONIA AND DENTIN SURFACE
dc.title.alternativeMonolitik Zirkonya Materyalinin Dentine Bağlanma Dayanımı Üzerine Farklı Tür Asit Yüzey Uygulamalarının Etkilerinin Araştırılması
dc.typeArticle

Dosyalar