Effect of Maleic Anhydride Pretreatment on Tensile Bond Strength of a Silicone Soft Liner to a Denture Base Polymer

dc.contributor.authorDemir, Hakan
dc.contributor.authorSoygun, Koray
dc.contributor.authorDogan, Arife
dc.contributor.authorKeskin, Selda
dc.contributor.authorDogan, Orhan Murat
dc.contributor.authorBolayir, Giray
dc.date.accessioned2019-07-27T12:10:23Z
dc.date.accessioned2019-07-28T10:05:05Z
dc.date.available2019-07-27T12:10:23Z
dc.date.available2019-07-28T10:05:05Z
dc.date.issued2011
dc.departmentFakülteler, Diş Hekimliği Fakültesi, Klinik Bilimler Bölümüen_US
dc.description.abstractPurpose: To determine the effect of resin surface treatment with dissolved maleic anhydride in butanone added into primer on the tensile bond strength between an acrylic denture base resin and a silicone soft liner. Materials and Methods: To test tensile bond strength, standard dumbbell-shaped acrylic specimens were prepared. Five experimental groups, including the control, were tested (n = 5). Maleic anhydride solutions prepared in butanone at concentrations of 1%, 5%, 10% or 20% were then mixed with 1 ml of Primo adhesive and the mixtures were applied onto the resin bonding surfaces. Silicone liner material was applied to resin surfaces in the conventional manner. Tensile bond strength of the specimens was measured in a universal testing machine. Fractured surfaces were observed under the scanning electron microscope, and resulting chemical changes with the solutions used were analyzed spectroscopically. Results: The highest bond strength value was obtained for the group treated with 5% maleic anhydride (2.53 +/- 0.48 MPa); the lowest value was for the group treated with 20% maleic anhydride (1.59 +/- 0.29 MPa). Mixed failure was the dominant type seen in the experimental groups. Spectroscopic analysis showed the interaction of the anhydride carbonyl groups with the Primo primer. Conclusion: The treatment of resin surfaces with maleic anhydride added to Primo adhesive effectively increased bond strength between silicone soft liner and denture base resin.en_US
dc.identifier.doi10.3290/j.jad.a19817en_US
dc.identifier.endpage487en_US
dc.identifier.issn1461-5185
dc.identifier.issn1757-9988
dc.identifier.issue5en_US
dc.identifier.pmid21246070en_US
dc.identifier.scopus2-s2.0-84856388210en_US
dc.identifier.scopusqualityQ1
dc.identifier.startpage481en_US
dc.identifier.urihttps://dx.doi.org/10.3290/j.jad.a19817
dc.identifier.urihttps://hdl.handle.net/20.500.12418/9451
dc.identifier.volume13en_US
dc.identifier.wosWOS:000296110200013en_US
dc.identifier.wosqualityQ3
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.indekslendigikaynakPubMeden_US
dc.language.isoenen_US
dc.publisherQUINTESSENCE PUBLISHING CO INCen_US
dc.relation.ispartofJOURNAL OF ADHESIVE DENTISTRYen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectPMMAen_US
dc.subjectsilicone soft lineren_US
dc.subjecttensile bondingen_US
dc.subjectSEMen_US
dc.subjectFTIRen_US
dc.subjectmaleic anhydrideen_US
dc.titleEffect of Maleic Anhydride Pretreatment on Tensile Bond Strength of a Silicone Soft Liner to a Denture Base Polymeren_US
dc.typeArticleen_US